I am building a fence for a display the company I work for is setting up at the Southern Ideal Home Show here in Raleigh. I have found a source for kiln dried after treating (KDAT)pressure treated lumber. I want to use it to minimize twisting and bowing, and to allow it to be painted sooner. I have two questions, as I have never worked with KDAT lumber. First should I use the same type of fasteners for normal wet ACQ PT lumber- Deckmate or something like that? Second, I can't get 6X6's in KDAT, so I'll have to go with regular juicy lumber, how long should I wait to paint them, and what type of paint would ya'll recommend. Thanks, for your thoughts and advice. Dave:smile: